Conformal Coating Cross Contamination
We apply 3 different types of conformal coating and cure them all in a single oven. We believe we are experiencing cross contamination.
Ask the Experts

View the Expert comments below.
,{url:'http://www.circuitinsight.com/videos/experts_final.mp4'}], clip:{autoBuffering:true, autoPlay:true, scaling:'scale' } }).ipad();

Arranged via association with Circuitnet..
See the Expert Panel | Submit A Questions | Join the Panel
Ask the Experts Question
Ask the Experts
Conformal Coating Cross Contamination
We apply 3 different types of conformal coating: Acrylic, Polyurethane and Silicone. We use designated dispensing systems for each, but cure them all in a single oven.

We believe we are experiencing cross contamination. If we purchase a second curing oven, which two coatings would be best to cure in the same oven?
A. K.
Expert's Panel Responses

Silicone is certainly the material most likely to cause problems if contaminating other product since it can cause problems with dewetting and adhesion. I would therefore recommend you use one oven for silicone and the other for the acrylic and polyurethane.

These two can share an oven with no problems providing you avoid any material physically dripping onto other assemblies.

image
Bryan Kerr
Principal Engineer - CMA Lab
BAE Systems
Bryan Kerr has 35 years experience in providing technical support to PEC assembly manufacturing. His experience ranges from analysis of materials and components to troubleshooting and optimizing, selecting reflow, cleaning, coating and other associated processes.

Acrylic and Polyurethane.

image
Wayne Wagner
President
Krayden Inc.
Wayne Wagner has over 25 years in the conformal coating industry and is the president of Krayden Inc., a leading distributor of engineered materials.

I would cure the silicone coating LAST and in its own oven. Urethane and acrylic are fine in the same oven...silicones are great materials, but traces can contaminate surfaces beyond our belief!

Jim Williams
Chairman
Polyonics, Inc.
Jim Willimas is a PhD Chemist in Polymers and Materials Science. He specialize in printing, cleaning, inks, and coatings used in electronics manufacturng operations. Williams has more than 30 years experience.

The short answer is, keep the Acrylic and Polyurethane on one line and the Silicone on a dedicated line.

Silicone will generally contaminate the board surface causing de-wetting when applying Acrylic and Polyurethane coatings.

I would suggest having the silicone line in another room or sealed area !

For information on which coatings to use for specific applications contact your coating supplier.

image
Chris Palin
European Manager
HumiSeal
Chris Palin is currently managing European sales and support for HumiSeal Conformal Coatings. His expertise is in test & reliability, solder technology, power die attach and conformal coating.
Generally, for conformal coating  you shouldn't see defects from  cross contamination in the oven from coatings based upon acrylic and polyurethane resins or their hybrids.   

The problems come with silicone materials. This is due to most coatings not liking to stick to silicone residues so any cross contamination through handling or application could be a problem.  

If you can avoid mixing silicone conformal coatings with other materials its generally better. Or, develop really good housekeeping and process controls. 
image
Lee Hitchens
Owner
SCH Technologies
Lee has worked within the conformal coating and electronics industry for over 18 years. His work includes scientific research into long term reliability of electronics, technical sales of conformal coating materials and equipment, owner of SCH Technologies, a conformal coating service in the UK, a member of the Diamond Coating Solutions Group, a global liquid conformal coating and Parylene coating service solutions provider, a founding member of Nexus3c, Conformal Coating Centre and a partner of Thin Film Partners.
Submit A Comment

Comments are reviewed prior to posting. Please avoid discussion of pricing or recommendations for specific products. You must include your full name to have your comments posted. We will not post your email address.

Your Name


Company


E-mail


Country


Comments


Authentication

Please type the number displayed into the box. If you receive an error, you may need to refresh the page and resubmit the information.



Related Programs
bullet Conformal Coating in Nitrogen Environment
bullet Conformal Coating Recommendation
bullet Why Uneven Conformal Coating?
bullet Jetting Fine Lines onto 2D and 3D Electronic Packages
bullet Aerosol Jet Printing of Conductive Epoxy for 3D
bullet Lower Temperature Solder Joint Encapsulant
bullet How To Verify Cleanliness After Rework and Prior to Re-coating?
bullet Thermally, Electrically Conductive Adhesive to Control Heat in PCBs
bullet Improving Reliability Through HALT and HASS Testing
bullet Conformal Coating over No Clean Flux
More Related Programs